
High-Temperature Optical Contact Angle Analyzer
The GFT-II-16 optical contact angle analyzer measures the wetting behavior and contact angle of materials at elevated temperature by transmission projection, imaging a specimen as it is heated, melted and dropped onto a substrate under vacuum or protective atmosphere. It covers room temperature to 1,700 °C, with continuous use below 1,600 °C, for metals, inorganic compounds and their mixtures through sintering, softening, melting and liquefaction.




